The main raw materials of SmCo permanent magnets are samarium and cobalt rare earth elements. SmCo magnet is the alloy magnet which produced through Power Metallurgy technology that is made into a blank by Melting, Milling, Compression Molding, Sintering, and Precision Machining.
MAGNETIC PROPERTY PARAMERERS OF SINTERED SM2CO17 | ||||||||||
Grade |
Br | Hcb | Hcj | (BH)max | Tc |
Tw | a(Br) | a(HcJ) | ||
Typical Value |
Min Value |
Min Value |
Min Value |
Typical Value |
Min Value |
Max Value |
Typical Value |
Typical Value |
||
[T] | [T] | [kA/m] | [kA/m] | [kJ/m3] | [ºC] |
[°ºC] |
[%/ºC] |
[%/°ºC] |
||
[KGs] | [KGs] | [KOe] | [KOe] | [MGOe] | ||||||
SmCo24H |
0.99 | 0.96 | 692 | 1990 | 183 | 175 | 820 |
350 |
-0.03 |
-0.2 |
9.9 | 9.6 | 8.7 | 25 | 23 | 22 | |||||
SmCo24 |
0.99 | 0.96 | 692 | 1433 | 183 | 175 | 820 |
300 |
-0.03 |
-0.2 |
9.9 | 9.6 | 8.7 | 18 | 23 | 22 | |||||
SmCo26H |
1.04 | 1.02 | 750 | 1990 | 199 | 191 | 820 |
350 |
-0.03 |
-0.2 |
10.4 | 10.2 | 9.4 | 25 | 25 | 24 | |||||
SmCo26 |
1.04 | 1.02 | 750 | 1433 | 199 | 191 | 820 |
300 |
-0.03 |
-0.2 |
10.4 | 10.2 | 9.4 | 18 | 25 | 24 | |||||
SmCo26M |
1.04 | 1.02 | 676 | 796-1273 | 199 | 191 | 820 |
300 |
-0.03 |
-0.2 |
10.4 | 10.2 | 8.5 | 10-16 | 25 | 24 | |||||
SmCo261 |
1.04 | 1.02 | 413 | 438-796 | 199 | 191 | 820 |
250 |
-0.03 |
-0.2 |
10.4 | 10.2 | 5.2 | 5.5-10 | 25 | 24 | |||||
SmCo28H |
1.07 | 1.04 | 756 | 1990 | 215 | 207 | 820 |
350 |
-0.03 |
-0.2 |
10.7 | 10.4 | 9.5 | 25 | 27 | 26 | |||||
SmCo28 |
1.07 | 1.04 | 756 | 1433 | 215 | 207 | 820 |
300 |
-0.03 |
-0.2 |
10.7 | 10.4 | 9.5 | 18 | 27 | 26 | |||||
SmCo28M |
1.07 | 1.04 | 676 | 796-1273 | 215 | 207 | 820 |
300 |
-0.03 |
-0.2 |
10.7 | 10.4 | 8.5 | 10-16 | 27 | 26 | |||||
SmCo28L |
1.07 | 1.04 | 413 | 438-796 | 215 | 207 | 820 |
250 |
-0.03 |
-0.2 |
10.7 | 10.4 | 5.2 | 5.5-10 | 27 | 26 | |||||
SmCo30H |
1.1 | 1.08 | 788 | 1990 | 239 | 222 | 820 |
350 |
-0.03 |
-0.2 |
11.0 | 10.8 | 9.9 | 25 | 30 | 28 | |||||
SmCo30 |
1.1 | 1.08 | 788 | 1433 | 239 | 222 | 820 |
300 |
-0.03 |
-0.2 |
11.0 | 10.8 | 9.9 | 18 | 30 | 28 | |||||
SmCo30M |
1.1 | 1.08 | 676 | 796-1273 | 239 | 222 | 820 |
300 |
-0.03 |
-0.2 |
11.0 | 10.8 | 8.5 | 10-16 | 30 | 28 | |||||
SmCo301 | 1.1 | 1.08 | 413 | 438-796 | 239 | 222 | 820 | 250 | -0.03 | -0.2 |
11.0 | 10.8 | 5.2 | 5.5-10 | 30 | 28 | |||||
SmCo30L |
1.1 | 1.08 | 413 | 438-796 | 239 | 222 | 820 |
250 |
-0.03 |
-0.2 |
11.0 | 10.8 | 5.2 | 5.5-10 | 30 | 28 | |||||
SmCo32 |
1.12 | 1.1 | 796 | 1433 | 255 | 230 | 820 |
300 |
-0.03 |
-0.2 |
11.2 | 11.0 | 10 | 18 | 32 | 29 | |||||
SmCo32M |
1.12 | 1.1 | 676 | 796-1273 | 255 | 230 | 820 |
300 |
-0.03 |
-0.2 |
11.2 | 11.0 | 8.5 | 10-16 | 32 | 29 | |||||
SmCo32L |
1.12 | 1.1 | 413 | 438-796 | 255 | 230 | 820 |
250 |
-0.03 |
-0.2 |
MAGNETIC PROPERTY PARAMETERS OF SINTERED SMCO5 | ||||||||||
Grade |
Br | Hcb | Hcj | (BH)max | Tc |
Tw | a(Br) | α(HcJ) | ||
Typical Value | Min Value |
Min Value |
Min Value | Typical Value | Min Value |
Max Value | Typical Value | Typical Value | ||
T (KGs) |
T (KGs) |
kA/m (KOe) |
kA/m (KOe) |
kJ/m3 (MGOe) |
[°ºC] |
[°ºC] |
[%/°ºC] |
[%/°ºC] |
||
SmCo16 |
0.83 | 0.81 | 620 | 1274 | 127 | 119 | 750 |
250 |
-0.04 |
-0.3 |
8.3 | 8.1 | 7.8 | 16 | 16 | 15 | |||||
SmCo18 |
0.87 | 0.84 | 645 | 1274 | 143 | 135 | 750 |
250 |
-0.04 |
-0.3 |
8.7 | 8.4 | 8.1 | 16 | 18 | 17 | |||||
SmCo20 |
0.92 | 0.89 | 680 | 1274 | 159 | 151 | 750 |
250 |
-0.04 |
-0.3 |
9.2 | 8.9 | 8.5 | 16 | 20 | 19 | |||||
SmCo22 |
0.95 | 0.93 | 710 | 1274 | 167 | 159 | 750 |
250 |
-0.04 |
-0.3 |
9.5 | 9.3 | 8.9 | 16 | 21 | 20 | |||||
SmCo24 |
0.98 | 0.96 | 730 | 1194 | 183 | 175 | 750 |
250 |
-0.04 |
-0.3 |